| STANDAARD | UNS | WNR. | AFNOR | NL | JIS | BS | GOST |
|---|---|---|---|---|---|---|---|
| RVS 304 | S30400 | 1.4301 | Z7CN18-09 | X5CrNi18-10 | SUS 304 | 304S31 | 08Х18Н10 |
| RVS 304L | S30403 | 1.4306/1.4307 | Z3CN18-10 | X2CrNi18-9 / X2CrNi19-11 | SUS304L | 304S11 | 03Х18Н11 |
| RVS 304H | S30409 | 1.4301 | - | - | - | - | - |
Chemische samenstelling van roestvrijstalen 304/304L/304H buizen en buizen
| C | Mn | Si | P | S | Cr | Ni | N | |
|---|---|---|---|---|---|---|---|---|
| 304 | 0,07max | 2,0max | 0,75max | 0,045max | 0,03max | min: 18,0 max: 20,0 | min: 8,0 max: 10,5 | - |
| 304L | 0,03max | 2,0max | 0,75max | 0,045max | 0,03max | min: 18,0 max: 20,0 | min: 8,0 max: 12,0 | Maximaal 0,10 |
| 304H | min: 18.0 maximaal: 20,0 |
min: 8,0 maximaal: 10,5 |
min: 0,04 maximaal:0,10 |
0.75 maximaal |
2.0 maximaal |
0.045 maximaal |
0.03 maximaal |
0.10 maximaal |
Mechanische eigenschappen van roestvrijstalen 304/304L/304H buizen en buizen
| Cijfer | Treksterkte ksi (min) | Opbrengststerkte 0,2% ksi (min) | Verlenging % | Hardheid (Brinell) MAX | Hardheid (Rockwell B) MAX |
|---|---|---|---|---|---|
| 304 | 75 | 30 | 40 | 201 | 92 |
| 304L | 70 | 25 | 40 | 201 | 92 |
| 304H | 75 | 30 | 40 | 201 | 92 |