ASTM A179 Carbon Steel Seamless Heat Exchanger Tube

Oct 23, 2025

Laat een bericht achter

ASTM A179 and ASME SA179 steel pipe covers thin-walled, seamless, cold-drawn, low-carbon steel tubing used in tubular heat exchangers, condensers, and similar heat transfer equipment.
We are a specialized manufacturer and supplier of ASTM A179 and ASME SA179 heat exchanger tubing. ASTM A179 carbon steel tubing offers durability, efficient heat transfer, and suitability for low-pressure applications. Key properties include a tensile strength of at least 325 MPa, a yield strength of at least 180 MPa, and a Rockwell hardness (HRB) not exceeding 72. ASTM A179 and ASME SA179 cover tubing with outside diameters ranging from 1/8 to 3 inches (3.2 to 76.2 mm).

 

ASTM A179 Carbon Steel Seamless Heat Exchanger Tube

 

ASTM A179,ASME SA179 Seamless Heat-Exchanger and Condenser Tubes Quick Details
Manufacture:Seamless process ,cold drawn.
Wall thickness(WT): 2.0 mm--12.7 mm.
Outer diameter (OD): 12.7mm--76.2 mm
Length: 6M or specified length as required.



Delivery: 7-15 days after payment
Surface: Tubes will be varnished (Outside only) to prevent rust.
Marking: Standard + Steel Grade + Size + Heat No + Lot No

 

 

Chemical Composition of ASTM A179,ASME SA179 Seamless Heat-Exchanger and Condenser Tubes

C P S
ASTM A179 0.06-0.18 <= 0.25 0.27-0.63 <=0.035 <=0.035


Mechanical Propertie of ASTM A179,ASME SA179 Seamless Heat-Exchanger and Condenser Tubes

ASTM A179
>=325
>=180
>=35
<=72

 




in. [mm]
Cut Length,in. [mm]
Seamless, cold-finished Under 2 [50.8] 1 ⁄ 8 [3] 0 [0]
2 [50.8] and over 3 ⁄ 16 [5] 0 [0]
2 [50.8] and over 3 ⁄ 16 [5] 0 [0]

 


ASTM A179,ASME SA179 seamless cold-drawn low-carbon steel tubes for tubular heat exchangers, condensers, and similar heat transfer apparatus.

info-1-1

 


Finished tubes shall be free of scale. A slight amount of oxidation will not be considered as scale.


In addition to the marking prescribed in Specification A450/A450M, the marking shall include the name and order number of the purchaser.
Note: Material furnished under ASTM A179,ASME SA179 conform to the applicable requirements of the current edition of Specification A450/A450M.